Many injection molding manufacturers will communicate with customers about the problem that the precision of injection molding thread does not meet the standard when making high-precision threads. They are eager to know if there is any way to solve this problem.
Because plastic is inferior to metal in terms of strength and stiffness, processing plastic threads by manufacturing metal threads must fail to meet the requirements. The threads of the outer ring of the plastic thread will have the risk of cracking or deformation. To avoid this problem, a step with a depth of 0.2-0.8MM should be set at the beginning of the thread; In addition, the end of the thread should be about 0.2MM away from the bottom.
Similarly, the starting end should also maintain a clearance of more than 0.2MM from the top surface, and the starting end and end of the external thread should not suddenly start and end, and excessive parts should be left. In addition, the injection molding manufacturer should pay attention to the size of the thread itself. Its diameter should not be too small, and the fitting length should not be too long, otherwise, the strength of the threaded connection will be reduced.